SnO2 nanotubes fabricated using electrospinning and atomic layer deposition and their gas sensing performance

SnO2 nanotubes fabricated using electrospinning and atomic layer deposition and their gas sensing performance

저자

Won-Sik Kim, byoung-Sun Lee, Dai-Hong Kim, Hong-Chan Kim, Woong-Ryeol Yu, Seong-Hyeon Hong

저널 정보

Nanotechnology

출간연도

2010

Won-Sik Kim, byoung-Sun Lee, Dai-Hong Kim, Hong-Chan Kim, Woong-Ryeol Yu, Seong-Hyeon Hong, “SnO2 nanotubes fabricated using electrospinning and atomic layer deposition and their gas sensing performance” Nanotechnology 21 245605(7pp) (2010)