Brookite TiO2 Thin Film Epitaxially Grown on (110) YSZ Substrate by Atomic Layer Deposition

Brookite TiO2 Thin Film Epitaxially Grown on (110) YSZ Substrate by Atomic Layer Deposition

저자

Dai-Hong Kim, Won-Sik Kim, Sungtae Kim, and Seong-Hyeon Hong*

저널 정보

ACS Applied Materials & Interfaces

출간연도

2014

Dai-Hong Kim, Won-Sik Kim, Sungtae Kim, and Seong-Hyeon Hong*, “Brookite TiO2 Thin Film Epitaxially Grown on (110) YSZ Substrate by Atomic Layer Deposition” ACS Appl. Mater. Interfaces 6 (2014) 11817−11822